Product Specifications

Temperature Range-100°C to 725°C
Heating Rate1000°C/s
Cooling Rate500°C/s
Sensitivity0.1mW
Sample Size50mg
Dimensions500x300x200 mm
UsagePolymer crystallization and reorganization analysis, analysis of thermally induced transitions, chemical process analysis
FeaturesFast heating, High resolution, Polymer analysis, Precise results, Wide temperature range, Easy operation

Product Overview

Key Features

As per the requirements of the customers, we are engaged Distributor, Supplier, Trading Company of Flash Differential Scanning Calorimeter in Secunderabad, Telangana, India. The instrument can analyze reorganization processes that were previously impossible to measure. The ultra-high heating and cooling rates add a new dimension to the study of thermally induced physical transitions and chemical processes, for example, the crystallization and reorganization of polymers.

Company Details

V. M. Sciences, Established in 2000 at Secunderabad in Telangana, is a leading Supplier,Trading Company of Testing & Measuring Equipment in India. V. M. Sciences is one of Trade India's verified and trusted sellers of listed products. With extensive experience in supplying and trading Flash Differential Scanning Calorimeter, V. M. Sciences has made a reputed name for itself in the market with high-quality Advanced Latest Technology Reflection Densitometer, Densitometers, Dry Sieve Test Apparatus, etc.
Focusing on a customer-centric approach, V. M. Sciences has a pan-India presence and caters to a huge consumer base throughout the country. Buy Testing & Measuring Equipment in bulk from V. M. Sciences at Trade India quality-assured products.

Business Type

Supplier, Trading Company

Establishment

2000

Working Days

Monday To Sunday

Related Products

Explore Related Categories

More Products From This Seller

Seller Details

Secunderabad, Telangana

Product Manager

Mr. Prasanna Kumar Sistia

Address

Plot No. 35, H. No. 3-6/1, Ayodhya Center, Kandlakoya, HAL Officers Colony, Old Bowenpally, Secunderabad, Telangana, 501401, India

calorimeter in Secunderabad

Report incorrect details

Compare With Similar Products

Buyer Feedback

3

Minimum Order Quantity

1 Set/Sets

1 Piece/Pieces

Payment Terms

Letter of Credit (L/C), Telegraphic Transfer (T/T)

Cash on Delivery (COD), Cash in Advance (CID), Cheque, Cash Advance (CA)

Supply Ability

3-4 sets Per Day

10-15 Per Week

Delivery Time

25 Days

10-15 Days

Packaging Details

wooden case, fumigated

Wooden Box

Main Export Market(s)

Asia, Australia, Central America, North America, South America, Eastern Europe, Western Europe, Middle East, Africa

South America, Western Europe, Asia, Australia, North America, Eastern Europe, Africa, Central America, Middle East

People Also Viewed